Of the specimens after carburizing and hardness of the composition. XRD analysis showed that the carburizing, the sample surface there is a clear TiC phase; fracture surface analysis can obviously see a layer of sediment. On the surface hardness after carburizing carburizing after tests found samples of the surface hardness increased 5 to 6 times. Successive points of cross section through the hardness test can probably determine the thickness of carburized layer. At a certain temperature and holding time, (eg under 950 ℃ for 3h), diffusion layer can reach about 100um, and substantial.